Product Description of Aluminum Silicate Ramming Material With Factory Price
Aluminum silicate ramming material is made of pure raw materials with low iron and low impurity content through reasonable grading and high efficiency admixture. It has high fire resistance, good abrasion resistance, strong thermal shock resistance, strong corrosion resistance and other excellent characteristics. It can be divided into different materials according to the raw materials used.
Product Specificaton of Aluminum Silicate Ramming Material With Factory Price
Элемент | Alumina-Silicon | Silicon- Carbide | Zirconium Chrome Corundum | ||||
KSL-1 | KSL- | KSL- | KSL- | KSL- | KSL- | KSL- | |
Al2O3 % | ≥65 | ≥75 | ≥85 | / | / | / | ≥80 |
SiC % | / | / | / | ≥40 | ≥60 | ≥70 | / |
Cr2O3 % | / | / | / | / | / | / | ≥3 |
ZrO2 % | / | / | / | / | / | / | ≥2 |
Bulk Density g/cm3 110℃×24h | ≥2.5 | ≥2.7 | ≥2.8 | ≥2.4 | ≥2.5 | ≥2.6 | ≥2.8 |
Скорость постоянного линейного изменения % 1000℃×3h | -0.4~0 | -0.5~0 | -0.5~0 | -0.4~0 | -0.5~0 | -0.6~0 | -0.6~0 |
Cold Crushing strength MPa 1000℃×3h |
≥70 | ≥80 | ≥90 | ≥60 | ≥70 | ≥80 | ≥90 |
Wear resistance at room temperature cm3 1000℃×3h | ≤7 | ≤6 | ≤5 | ≤7 | ≤6 | ≤5 | ≤5 |
Thermal shock resistance 1000℃ water cooling cycle 1000℃×3h Fired | ≥30 | ≥30 | ≥25 | ≥30 | ≥35 | ≥40 | ≥30 |
Plasticity Index % | 15~55 | ||||||
Thermal conductivity W/(м·К) 1000℃ | 1.1~1.6 | 1.6~2.0 | 3~5 | 5~7 | 6~8 | 2~3 |